100 homemade LDJ-240 chloroprene rubber, 18 styrene butadiene styrene block copolymer and 700 parts of toluene were mixed with 700 parts of toluene, and heated by salt bath, stirring and melting, and stirring slowly into 80 portions of methyl methacrylate (or n-butyl methacrylate), which had dissolved 0.7 phr, and stirred up to 95 degrees C, when the viscosity was heated. When 0.7~0.9 mooring, 1.2 hydroquinone inhibitors are added immediately. Heat preservation and stirring for 4 hours, stop heating, and cool naturally. At the same time, 15 terpene phenolic resins and 1 antiaging agents are added to cool to room temperature. In order to adjust the viscosity, a small amount of toluene can be added, and the amber color finished product has a solid content of 27-30%.
The three element graft adhesive is especially suitable for cold adhesion between PVC artificial leather / PVC artificial leather, PVC artificial leather / vulcanized natural rubber and so on. It can overcome the shortcoming of insufficient adhesion strength of two element graft adhesive to vulcanized natural rubber, and makes the adhesion strength of the latter up to 6 thousand and 900 Newton / M.
When used, the three component graft adhesive is the same as the two component graft adhesive, and the curing agent must be added with a curing time of 72 hours.